CHENILLE IRON ON INSTRUCTIONS

  • Use any fabric adhesive spray on the back of the patch.
  • Place the patch on the garment, and put a towel or fuzzy material on the surface of heat press.
  • Place the garment on the heat press machine, patch facing down.
  • Press the patch on 160 C / 320 F temperature for 15-20 time.

Heat Press:  Temperature 160 C / 320 F for 15-20 seconds
Iron: Adjustment temperature & time according to your fabric

EMBROIDERY IRON ON INSTRUCTIONS

  • Place the garment on the heat press machine with the patch.
  • Press the garment at 160 C/ 320 F temperature for 15 seconds.
  • Let the patch cool down before further handling.

Heat Press: Temperature 160 C/ 320 F for 15-20 seconds

Iron: Adjustment temperature & time according to your fabric

PVC IRON ON INSTRUCTIONS

  • Use adhesive spray on the back of the patch.
  • Place the patch on the garment.
  • Place the garment on the heat press machine, patch facing down.
  • Press the patch on 160 C/ 320 F temperature for 20-30 seconds.

Heat Press: Temperature 160 C/ 320 F for 15-20 seconds

Iron: Adjustment temperature & time according to your fabric

WOVEN IRON ON INSTRUCTIONS

  • Place the garment on the heat press machine with the patch.
  • Press the garment on 140 C/ 284 F temperature for 20 seconds.
  • Let the patch cool down before further handling.

Heat Press: Temperature 140 C/ 284 F for 15-20 seconds

Iron: Adjustment temperature & time according to your fabric

SUBLIMATION IRON ON INSTRUCTIONS

  • Place the garment on the heat press machine with the patch.
  • Press the garment on 160 C/ 320 F temperature for 15 seconds.
  • Let the patch cool down before further handling.

Heat Press: Temperature 160 C/ 320 F for 15-20 seconds

Iron: Adjustment temperature & time according to your fabric

LEATHER IRON ON INSTRUCTIONS

  • Use adhesive spray on the back of the patch.
  • Place the patch on the garment.
  • Place the garment on the heat press machine, patch facing down.
  • Press the patch on 140 C/ 284 F temperature for 15-20 seconds.

Heat Press: Temperature 140 C/ 284 F for 15-20 seconds

Iron: Adjustment temperature & time according to your fabric